AISI 329 / 1.4460 STAINLESS STEEL

Status
Not open for further replies.

rajnad

Materials
Nov 7, 2011
7
Dear All,

Request to advise if AISI 329 or 1.4460 complies and can be certified as per NACE MR0175 or MR0103 Latest editions.

Please explain in details if possible.

Regards

[thanks]
 
Replies continue below

Recommended for you

Duplex stainless steel type 329 would meet NACE MR0175/ISO 15156-3 if the molybdenum concentration is at least 1.5 %.
 