Jun 21, 2012 #1 azzt Mechanical May 19, 2004 32 0 0 GB Hi I'm trying to find some creep rupture data at elevated temperatures for aisi 4340 steel at conditons other than normalized (which I already have). Ideally for material around about a HRC=45. Any help would be appreciated. Thanks allan
Hi I'm trying to find some creep rupture data at elevated temperatures for aisi 4340 steel at conditons other than normalized (which I already have). Ideally for material around about a HRC=45. Any help would be appreciated. Thanks allan
Jun 21, 2012 1 #2 metengr Materials Oct 2, 2003 15,478 0 0 US http://deepblue.lib.umich.edu/bitstream/2027.42/4320/5/bab3992.0002.001.pdf Upvote 0 Downvote
Jun 22, 2012 Thread starter #3 azzt Mechanical May 19, 2004 32 0 0 GB Thanks mentengr allan Upvote 0 Downvote