AL alloy Liquid Density 1

Status
Not open for further replies.

CastMetal

Mechanical
Jun 8, 2010
147
Does anyone know of a place to find liquid density of various alloys? Specifically AL 6061 in this case. If not any good ideas on how to measure it more precisely than simply marking a level on a ladle and finding final weight of an ingot poured at that level?
 
Replies continue below

Recommended for you

Smithells handbook,will give you the data.However,you can consider 2.43gms/cc for practical purposes.
 