Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Al Casting alloys 2

Status
Not open for further replies.

kenre

Mechanical
Joined
May 23, 2005
Messages
300
Im after info on available aluminium casting alloys in Australia. Google hasnt been of much use, Sims metals have given 4 alloys, but no data sheets or specifications.

I need to choose an alloy for model racing engine crankcases.

Strength, Stability, and crack resistance are high priorities.



Was told it couldnt be done, so
i went and did it!
 
AA 356-T6 is as good a place to start as any, and is a fairly common alloy. Sand cast is 30,000 psi min tensile.How big is this engine crankcase? Perhaps a CNC hog out of billet might be more feasible.
 
Swall, I keep reading about 356 T6, but to cross reference to whats available in Australia has been a fruitless search.

CNC would be ideal, but not having one myself, yet, and the lowish numbers to be produced make it too expensive per piece.




Was told it couldnt be done, so
i went and did it!
 
AA 365 is known as AC601 (primary alloy) or DA601 (secondary alloy) in Australia, and is standardized in AS 1874 Aluminium and aluminium alloys - Ingots and castings.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Primary means it was produced directly from aluminum-containing ore (bauxite) while secondary means it has been produced from recycled metal. Secondary generally has higher impurity levels (iron, zinc, etc.) which probably won't be an issue for your application. Most automotive blocks are now cast with secondary metal.
 
Thankyou once again.

Does anyone know where i can locate a listing of casting alloys? i dont want to settle for the first i see, as there maybe something more suited. Even Al/Li ???




Was told it couldnt be done, so
i went and did it!
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top