Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Alaska Yellow Cedar 5x5 and larger NDS supplement

Status
Not open for further replies.

SubtleNova

Structural
Apr 15, 2022
3
I see this thread but I'm unsatisfied with the answer:

NDS Supplement 2015 Table 4A lists Alaska Cedar AND Alaska Yellow Cedar for 2" - 4" thick. (page 33)
But, Table 4D only shows Alaska Cedar for 5"x5" and larger. (page 47)

The fact that table 4A lists them separate makes it seem like Alaksa Cedar is not the same as Alaska Yellow Cedar.
I'm used to listing AYC grade for 2x and 4x, but what do I list for 6x beams and columns?

I'm in the Pacific Northwest area, mainly Washington and Idaho.
 