a_wall_e
Aerospace
- Jan 6, 2021
- 2
Hello,
I had a question on how to best properly apply material properties to a given piece of metal. As an example of the question: say that there is an aluminum 7075-T73 plate 4 inches thick that is machined down to form a pocket, so that all thicknesses are now 1 inch thick. Would one need to use mechanical properties for the 4 inch thickness range or could one use the 1 inch material properties for structural analysis?
I had a question on how to best properly apply material properties to a given piece of metal. As an example of the question: say that there is an aluminum 7075-T73 plate 4 inches thick that is machined down to form a pocket, so that all thicknesses are now 1 inch thick. Would one need to use mechanical properties for the 4 inch thickness range or could one use the 1 inch material properties for structural analysis?