Can a welder weld SA 335 GR P-11 with SA335 GR P22 Filler.. if so, what is the referencing code section?

Pl. help

Alok
 
Replies continue below

Recommended for you

Yes, as long as there is a qualified WPS for doing so. It's F-No that's the essential variable for Welder Qualification - not A-No.
 
Most Codes and Standards do not recommend filler metals for weld joints, that is left up to the designer.
 