Jan 1, 2004 #1 stevea2 Mechanical Aug 5, 2003 6 0 0 US does anyone know the pulling temp of alumina silicate glass. when we pull the glass seems to be very thick and full of airlines. we are pulling from a crucible that holds about 90#s of glass cullet. and we cant seem to get the defects out
does anyone know the pulling temp of alumina silicate glass. when we pull the glass seems to be very thick and full of airlines. we are pulling from a crucible that holds about 90#s of glass cullet. and we cant seem to get the defects out