Jan 22, 2004 #1 julio Automotive Feb 18, 2002 6 0 0 FR Could someone give me datas on allowable surface pressure of aluminium under pressure of a tightened screw The material is die-cast aluminium ref : Al-Si8 Cu3Fe according ISO3522 A380.0 / SC84A according to ASTM B85
Could someone give me datas on allowable surface pressure of aluminium under pressure of a tightened screw The material is die-cast aluminium ref : Al-Si8 Cu3Fe according ISO3522 A380.0 / SC84A according to ASTM B85
Jan 22, 2004 1 #2 CoryPad Materials Apr 15, 2002 5,192 0 0 US This type of data is not published widely. The closest I have seen is this: G AlSi9Cu3, Werkstoffnummer 3.2163.01, R[sub]m[/sub] = 304 MPa, R[sub]p0,2[/sub] = 168 MPa, A[sub]5[/sub] = 4.5%, HB = 103, p[sub]G[/sub] = 383 MPa GD AlSi9Cu3, Werkatoffnummer 3.2163.05, R[sub]m[/sub] = 232 MPa, R[sub]p0,2[/sub] = 159 MPa, A[sub]5[/sub] = 2%, HB = 88, p[sub]G[/sub] = 367 MPa Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
This type of data is not published widely. The closest I have seen is this: G AlSi9Cu3, Werkstoffnummer 3.2163.01, R[sub]m[/sub] = 304 MPa, R[sub]p0,2[/sub] = 168 MPa, A[sub]5[/sub] = 4.5%, HB = 103, p[sub]G[/sub] = 383 MPa GD AlSi9Cu3, Werkatoffnummer 3.2163.05, R[sub]m[/sub] = 232 MPa, R[sub]p0,2[/sub] = 159 MPa, A[sub]5[/sub] = 2%, HB = 88, p[sub]G[/sub] = 367 MPa Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Jan 22, 2004 #3 mirekp Mechanical Sep 7, 2002 49 0 0 CZ For more info you can try the excellent material web http://www.matweb.com Searched materials are: http://www.matweb.com/search/SpecificMaterial.asp?bassnum=MAC385http://www.matweb.com/search/SpecificMaterial.asp?bassnum=MAC380 Mirekp Mechanical and engineering calculations http://www.mitcalc.com Upvote 0 Downvote
For more info you can try the excellent material web http://www.matweb.com Searched materials are: http://www.matweb.com/search/SpecificMaterial.asp?bassnum=MAC385http://www.matweb.com/search/SpecificMaterial.asp?bassnum=MAC380 Mirekp Mechanical and engineering calculations http://www.mitcalc.com