Hello,
I am looking to fabricate a lift device for use in cold weather (down to -45C). Aluminum 6061-T6 appears to be acceptable from the information I have, -45 will only make aluminum stronger (do not need to worry about brittleness like with steel).
Anyone have any knowledge of Aluminum and cold weather (down to -45C) being an issue?
Thanks in advance!
I am looking to fabricate a lift device for use in cold weather (down to -45C). Aluminum 6061-T6 appears to be acceptable from the information I have, -45 will only make aluminum stronger (do not need to worry about brittleness like with steel).
Anyone have any knowledge of Aluminum and cold weather (down to -45C) being an issue?
Thanks in advance!