Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Aluminum in Cold Weather, Cold Temperature Applications

Status
Not open for further replies.

AEng123

Mechanical
Nov 2, 2016
18
Hello,

I am looking to fabricate a lift device for use in cold weather (down to -45C). Aluminum 6061-T6 appears to be acceptable from the information I have, -45 will only make aluminum stronger (do not need to worry about brittleness like with steel).

Anyone have any knowledge of Aluminum and cold weather (down to -45C) being an issue?

Thanks in advance!
 
Replies continue below

Recommended for you

Well before Invar became a thing, they used to make LNG (-168C) tanks and pipes from Aluminium so -45 shouldn't be a big issue, but I guess there are different grades of /Aluminium.

Plenty of info about like this
Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Aluminum is used for exchangers in cryogenic exchangers for nat gas separation. I don't know temperatures ,but much lower than - 45C.
 