We're doing some machining to a beefy 6061-T6 extrusion and are VERY concerned about residual stresses in the material afterwards(as a result of extruding and machining). Two questions:
1. Any idea if dimensional creep is likely as a result of machined in stresses over the life of the part? For this application 5 micron is too much!
2. What heat treatment would remove residual stresses but preserve the T6 temper?
Thanks!
1. Any idea if dimensional creep is likely as a result of machined in stresses over the life of the part? For this application 5 micron is too much!
2. What heat treatment would remove residual stresses but preserve the T6 temper?
Thanks!