drukvat
Industrial
- Jan 10, 2008
- 7
We have Qualified X80 pipe to AISI 4130 flange acc to ASME lX With ABS witnessing Authority.
The Tube/Flange(21") is PWHT condition after welding. Now inspector says, that this procedure is not anymore
According ASME lX, because of the PWHT treatment,
The X80 Yield strength lowers the pipe mechanical properties to 550 Mpa after 4 hours.
This treatment we already did, because the 2hours is just giving us good PWHT properties, any way, if we must repair, we need to treat again. Does this inspector have right conclusion?
The Tube/Flange(21") is PWHT condition after welding. Now inspector says, that this procedure is not anymore
According ASME lX, because of the PWHT treatment,
The X80 Yield strength lowers the pipe mechanical properties to 550 Mpa after 4 hours.
This treatment we already did, because the 2hours is just giving us good PWHT properties, any way, if we must repair, we need to treat again. Does this inspector have right conclusion?