I have 304 stainless steel foil about 0.05 mm (0.002") thick. I dont have much more information . Sorry.
I wish to anneal foil so that it is easier to cold form small squares about 20x20 mm . Is there an easy to do this without having to send to heat treating facility? I have flame torch and high temperature thermocouple probes. I assume there would be more to it than heating to 1100C 2000F and cooling in hot sand.
thanks
I wish to anneal foil so that it is easier to cold form small squares about 20x20 mm . Is there an easy to do this without having to send to heat treating facility? I have flame torch and high temperature thermocouple probes. I assume there would be more to it than heating to 1100C 2000F and cooling in hot sand.