Has anyone the info at hand to state what the actual design temperature rating is for a 300# A105 type material.
 
Replies continue below

Recommended for you

What is your design temperature?

100° 740 psi
300° 655 psi
600° 570 psi

etc.
 
I wouldn't be inclined to go above 775 to 800 F, the onset of graphitization, even though B31.3 lists allowable stresses in tension for A105 up to 1100 F in Table A-1. The graphitization threshold in ASME B16.5 Table 2-1.1 is listed as 425 C (797 F), with an upper temperature limit of 538 C (1000 F). The corresponding flange ratings for 300# are 28.8 bar @ 425 C and 5.9 bar @ 538 C.