API-1104 Section 5.4.22 states;
When welding pipe of different base materials. The procedure for the higher strength base material group shall be used
for the qualification of welding procedures.
1. Can you please inform, if I am to weld X65 grade material (Group 'C') to X42 grade material (Group 'A') I have to qualify a
weld procedure on X65 to X65 material or can I qualify the weld procedure with X65 to X42 material.
I would have thought it better to qualify the weld procedure on X65 to X42 material as this would give mechanical results
which are a true representation of the actual materials to be welded.