GHFInspector
Petroleum
- Jun 15, 2011
- 8
When testing welder to API 1104, is the material an essential variable? Can I give them a 12" butt and branch test with Grade B STD wall pipe, 6010 downhill all the way and they be good for all thicknesses and diameters and grades? The reason why I'm asking is we are welding Grade B pipe all the way up to X70. I have 10 different WPS's but the only rods we are using are E6010, 7010 and 8010 (All group 1,2). Basically all essential variables are the same but the pipe grade's differ. Also, if this works out, since I have 10 different WPS's, would I choose one to test them on and only write the one tested on my WPQ or would I also input all procedures they are qualified for (All 10 WPS's) since they passed the initial test? As you can probably tell, I'm a newbie so all help is appreciated. Thanks.