Hey guys I'm looking for some guidance on running a welding procedure on api 2h gr50 to 316ss and it requires charpy it is to AWS d1.1. Or should I be looking in AWS d1.6? Help please.

Thanks in advance
Qcpeewee
 
Replies continue below

Recommended for you

Sorry to be brusque but you need to contact a local welding engineer.

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
 
Read the preface to AWS D1.1 - it is only valid for mild carbon steel, with thicknesses above that of sheetmetal. Thus it is impossible to use D1.1.
 