57
AR
Hi, I was wondering if is possible to make an API 579 S4 for a whole Pipeline. I've a situation of one Pipeline wich required thickness is 1mm below the average measured. Is possible make this kind of analysis? What another choice do I have?
 
Replies continue below

Recommended for you

Dear Maku,

Yes you can perform a Fitness For Service for general metal loss by API 579. Other choice is ASME B31G.

Kind regards
Fernando
 