Hi All,

As per our specification the required material grade is API 5CT T-95 PSL2

But, vendor will only be able to supply T-95 PSL1 instead of T-95-PSL2. What are the main differences between PSL-1 & PSL-2? Can we accept T-95 PSL1 ?

Regards

 
Hi All,
My previous post had a typo. here's the corrected one. i am waiting for responses.

As per our specification the required material grade is API 5CT T-95 PSL2.
But, vendor will only be able to supply T-95 PSL1 instead of T-95-PSL2. What are the main differences between PSL-1 & PSL-2? Can we accept T-95 PSL1 ?

Regards
 
Why don't you get hold of a copy of API Spec 5CT and review the differences for yourself? Then you will be able to make a judgement based on the perceived quality needs of the product for your specific application. It's no use pleading for assistance on a forum from those of us who have no clue about what you intend to do with the items.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Thanks for your great advice.

Regards
 
A little history and caution : T 95 was the first grade of API OCTG that could not be made by every US mill. When it was first approved no mill in north america could make it ; they could not pass the NACE test. I don't have a current 5 CT but if you really need T 95 , I would want a mill that can pass a NACE test( per heat, and heat-treat lot) whatever PSL that requires .
 