Dear Friends
Applicable Codes - ASME Section IX & ASME B31.3
Weld Process - GTAW / SMAW
Test Positions - 2G & 5G separately
Base Material - API 5L X65Q x 30mm thk.
I have to know acceptable Min. / Max. Hardness Value after PWHT. Client Spec refer NACE MR 0175 which i dont have
Can shine some light on this?
Thanks