mancini
Mechanical
- Mar 6, 2003
- 29
I have worked in an API 650 tank design, carbon steel ASTM A 36 and the maximum normal fluid operation temperature is 194 F (90 C).
Is it a must to consider the appendix M from API 650 if the design temperature is 230 F (110 C)?
This design temperature, in our case, is not a usual temperature that can occur only in a process extreme condition, which is possible to occur only if there is a failure in other equipment's or if there is an operation mistake.
Thanks.
Is it a must to consider the appendix M from API 650 if the design temperature is 230 F (110 C)?
This design temperature, in our case, is not a usual temperature that can occur only in a process extreme condition, which is possible to occur only if there is a failure in other equipment's or if there is an operation mistake.