JeffLester
Mechanical
I'm reviewing the repair plan for an API riveted tank. The plan calls for the replacement of various shell sections including some intersections of horizontal and vertical seams. The shell is 3/8" CS. I've reviewed 653 and have some preliminary issues with how this replacement would be done. Any thoughts on this would be greatly appreciated.