- Feb 3, 2005
- 11
We have firetested a Carbon Steel valve to the above std. My belief is that testing this valve ONLY qualifies us for valves as listed in ASME B16.34 Group 1 of Table 1. The problem we have is that we have a contract where have supplied Duplex Steel Valves as tested to API607, if my understanding is correct we are required to test a Stainless steel to cover us for this valve material under ASME B16.34 Groups 2 and 3 of Table 1. Basically testing carbon steel only covers us for "ferrite" steels ie Table 1 Group 1.
Can anyone confirm or give advice.