Good Day expert,

Can anyone help me to know the applicable welding consumable for SUH409L+SUH409L (cold rolled). any reference?
SUH409L - 10.5~11.75 Cr
A number - 7
Ferritic type

your answers are very much appreciated.
thank you in advance

 
Replies continue below

Recommended for you

thank you for your grat answer @metengr.
any reference sir?
HOw about for GMAW or FCAW process?
 
Mark, what does your consumable supplier suggest?
Look in the manuals from Miller and Lincoln.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 