Hi. I need your help again,
The cuestion is as follow:
First:
In accordance to API-1104, the welding procedure can be qualified by "Welding of Test Joints-Butt Welds" or "Welding of Test Joints-Fillet Welds".
Moreover, a major change in joint design constitute an essential variable.
The cuestion: Can we weld T or Lapped fillet joints with a WPS qulified by "Welding of Test Joints-Butt Welds" ??
Second:
For ASME B31.4, the ARC BURN on the pipes surface shall be repaired because this is a stress concentrator.
The cuestion: Should be considered a temporary T or Lapped fillet weld on the pipe surface, as much or more harmful than the arc burn ??
(temporary weld made with the above described procedure qulified by "Welding of Test Joints-Butt welds")
Thanks in advance for your comments or help about.
The cuestion is as follow:
First:
In accordance to API-1104, the welding procedure can be qualified by "Welding of Test Joints-Butt Welds" or "Welding of Test Joints-Fillet Welds".
Moreover, a major change in joint design constitute an essential variable.
The cuestion: Can we weld T or Lapped fillet joints with a WPS qulified by "Welding of Test Joints-Butt Welds" ??
Second:
For ASME B31.4, the ARC BURN on the pipes surface shall be repaired because this is a stress concentrator.
The cuestion: Should be considered a temporary T or Lapped fillet weld on the pipe surface, as much or more harmful than the arc burn ??
(temporary weld made with the above described procedure qulified by "Welding of Test Joints-Butt welds")
Thanks in advance for your comments or help about.