does any body information about architectural precast elements, ie, coloured concrete, exposed agregate, acid surface, hydrofobic products, surface resin, etc.
 
Replies continue below

Recommended for you

See the British Concrete Society,<br>
Technical Report No 13, published March 1977<br>
ISBN 0 7210 1060 1.<br>
Chapters 6 and 8 have some info on special finishes.<br>
Also various chemical businesses (eg Bayer) have literature on colourings for concrete.
 