Dec 7, 2014 #1 krishh07 Mechanical Dec 7, 2014 16 0 0 IN as per ASME Sex IX,if PQR done with P1 Gr1 to same,is it qualified for P1G1 and P1G2?please clarify Kind Regards M.K.Sridhar
as per ASME Sex IX,if PQR done with P1 Gr1 to same,is it qualified for P1G1 and P1G2?please clarify Kind Regards M.K.Sridhar
Dec 7, 2014 2 #2 gtaw Structural Feb 10, 2006 1,954 0 0 US Yes, if toughness is not a requirement of the construction code, i.e., Section I, Section VIII, B31.1, etc. No, if toughness testing is required per the construction code. Best regards - Al Upvote 0 Downvote
Yes, if toughness is not a requirement of the construction code, i.e., Section I, Section VIII, B31.1, etc. No, if toughness testing is required per the construction code. Best regards - Al