ASCE 41 Default Properties for Masonry include strength reduction factors

Status
Not open for further replies.

David Deck Guy

Structural
Aug 18, 2023
36
I was digging into the commentary on this section and noticed that it makes numerous references to having already applied strength reduction factors. These strength reduction factors are in line with TMS 402 (0.6 unreinforced, 0.9 reinforced).

Have I been applying double strength reduction factors this whole time, or do I need to apply them multiplicatively?