Ok, I'm in a pinch. I am with-out the ASME Section II. I need the allowable stress values for SA516-70 steel at 120 deg F. Most of my work involving the B&PV code has involved stainless steel (like 316L). I keep copies of the data in the submitted calculations, for stainless steel. However, due to a mix-up our Code was lent to another branch and I am having trouble contacting the person who has it. I did a quick calculation using the structural standy of .66Fy, but I'd like to double check that value at operating temperature.

 
Also, let me add any help would be greatly appreciated.
 
Sec. VIII Div. 1 2007 ed.
SA-516 Gr. 70 plate, 65 C, 138 MPa
notes G10, S1, T2, none of which apply at your temperature.
 
Ok, Thanks. I appreicate it.
 
SA516 Gr. 70 holds its room-temp strength up to 500°F. Derates start at 501°.
 