Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations The Obturator on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME B16.5-2003 Material Group 3.1 Nominal Designation 1

Status
Not open for further replies.

doct9960

Mechanical
Aug 15, 2006
618
ASME B16.5-2003 shows an incorrect "Nominal Designation" on Table 1A, Table 2-3.1, and Table F2-3.1

The correct nominal designation should be 35Ni–35Fe–20Cr–Cb
 
Good Catch! I found that the 1988, 1996, 1996/98a B16.5 standards all state 20Cr as well. It must have been missed in the 2003 Edition.

It does not appear that the committee has identified this error.. yet...or maybe they have and there is a plan to put into the 2007 B16.5?
I suggest you contact a member of the committee that approves errata to this standard. Here is a link to the committee where you will find the committee staff contact person: