Section 1.3 of ASME B16.9 specifies the following:
“Fabricated laterals and other fittings employing circumferential or intersection welds are considered pipe fabrication and are not within the scope of this Standard.”
If two halves of a large tee are forged then welded together with 100% radiography of the weld is there a way of allowing the Tee to remain compliant with ASME B16.9?
“Fabricated laterals and other fittings employing circumferential or intersection welds are considered pipe fabrication and are not within the scope of this Standard.”
If two halves of a large tee are forged then welded together with 100% radiography of the weld is there a way of allowing the Tee to remain compliant with ASME B16.9?