sziva
Mechanical
- Apr 28, 2011
- 3
Hello All,
I have some issues with the ASME B31.1 PWHT requirements.
Issue:
Table 132 contains the PWHT requirements based on material P-Nos (position) and Gr. Nos (grade).
The P-No is clearly defined for each material in Mandatory Appendix A. For instance A335 P22 material's P-No. is 5A.
The Gr. No. interpretation is unclear to me.
Staying with the same example. Appendix A - A335 pipe material for P-No 5A contains two grades starting with 2 : P21 and P22. I would assume, that the two different grades are interpreted as two grade numbers.
Here comes the twist. Back to table 132.
Table 132, P-No. 5A only mentions the requirement for Gr.No. 1. How should one understand this? Does Gr.No 1 refer to the first grade, P21?
What makes the picture more blurred is the example of material A335 P91. This material has a P-No. 5B and the only one grade of material A335 starting with 9 is P91 only. If I check again Table 132 for P-No. 5B, Gr. Nos. 1,2 are mentioned.
If someone familiar with ASME B31.1, please help me.
Thanks.
Regards,
LSZ
I have some issues with the ASME B31.1 PWHT requirements.
Issue:
Table 132 contains the PWHT requirements based on material P-Nos (position) and Gr. Nos (grade).
The P-No is clearly defined for each material in Mandatory Appendix A. For instance A335 P22 material's P-No. is 5A.
The Gr. No. interpretation is unclear to me.
Staying with the same example. Appendix A - A335 pipe material for P-No 5A contains two grades starting with 2 : P21 and P22. I would assume, that the two different grades are interpreted as two grade numbers.
Here comes the twist. Back to table 132.
Table 132, P-No. 5A only mentions the requirement for Gr.No. 1. How should one understand this? Does Gr.No 1 refer to the first grade, P21?
What makes the picture more blurred is the example of material A335 P91. This material has a P-No. 5B and the only one grade of material A335 starting with 9 is P91 only. If I check again Table 132 for P-No. 5B, Gr. Nos. 1,2 are mentioned.
If someone familiar with ASME B31.1, please help me.
Thanks.
Regards,
LSZ