I've been trying to find the definition of what material should be used for Curve A,B,C, and D on Fig. 323.2.2A. I reviewed Appendix A and Table A-1 and can't find any note that tells me which curve to use for A106/A333, and 1.25/2.25 Cr pipe. Can someone point the way for me? I guess the set up for the notes for this curve is different than the notes for Section VIII.
I've been trying to find the definition of what material should be used for Curve A,B,C, and D on Fig. 323.2.2A. I reviewed Appendix A and Table A-1 and can't find any note that tells me which curve to use for A106/A333, and 1.25/2.25 Cr pipe. Can someone point the way for me? I guess the set up for the notes for this curve is different than the notes for Section VIII.