I would like to understand ASME IX concerning welders qualification.
QW 350 gives essential variables. For SAW, P Number is an essantial variable and we have to see QW 403.18.
QW 403.18 gives “ a change from one P Number to any other P Number or……. exept as permitted in QW423, and QW 420.2.”
We have a welder qualified with a base metal P N°1.
Is it Qualified for P N°1 through PN°11?
Alternatively, is a welder qualified for a PN°11, qualified for PN°1?
I would like to understand the exeption.
Thank you for your answers
JL
QW 350 gives essential variables. For SAW, P Number is an essantial variable and we have to see QW 403.18.
QW 403.18 gives “ a change from one P Number to any other P Number or……. exept as permitted in QW423, and QW 420.2.”
We have a welder qualified with a base metal P N°1.
Is it Qualified for P N°1 through PN°11?
Alternatively, is a welder qualified for a PN°11, qualified for PN°1?
I would like to understand the exeption.
Thank you for your answers
JL