Cloya14
Petroleum
- Sep 16, 2014
- 17
I am trying to figure out if there is a limit on repairs of a weld joint before the HAZ needs to be cut out. Currently we repair a part for a customer about once a year and we continually have done this on that part about 8 times. Neither UG-78 or UW-38 cover anything on this so im stuck and would like input from the experts. Thanks in advance.