Dear Members,
Hope you are all well !
I am facing difficulty in finding the A-Number for a TIG rod Identified AS ( AWS A5.14| ERNiCr-3 ).I have to use it for welding of SS to C/S in a High Temperature Application. Checking our WPSs, I need to know the A-Number for that electrode to proceed
According to Table QW-442, ASME IX I need to compare the chemical composition with the table to know what A-No of weld metal is it.
Checking the table I found the max Ni % available is 37% While this rod (ERNiCr-3) has >67 & of Ni according to the manufacturer & AWS A5.14. I attached the tag on the rod box and the manufacturer data sheet.
Appreciating your help,
Thanks in advance.
Hope you are all well !
I am facing difficulty in finding the A-Number for a TIG rod Identified AS ( AWS A5.14| ERNiCr-3 ).I have to use it for welding of SS to C/S in a High Temperature Application. Checking our WPSs, I need to know the A-Number for that electrode to proceed
According to Table QW-442, ASME IX I need to compare the chemical composition with the table to know what A-No of weld metal is it.
Checking the table I found the max Ni % available is 37% While this rod (ERNiCr-3) has >67 & of Ni according to the manufacturer & AWS A5.14. I attached the tag on the rod box and the manufacturer data sheet.
Appreciating your help,
Thanks in advance.