ASME Sect. IX SA212 2

Status
Not open for further replies.

erssk

Materials
Jan 15, 2007
4
I know SA212 was superseded in 1962 by SA 515. Was SA212 a P1 gr1 material also.
 
Replies continue below

Recommended for you

SA212 is a P1 material. The group number will depend on tensile strength; therefore, the grade is also important.

Joe Tank
 