I am in the process of installing new sulfuric acid piping and storage system in a alumina production plant,and I would appreciate any guidance on material selection and the best pump to overcome a head of 50 feet, the ambient temp is about 40C.
 
Replies continue below

Recommended for you

B8K!

In our sulphuric acid plant we used to have centrifugal pumps made up of CF8M and with carbon steel piping.