Hi everybody!!!

I`m looking for the density, thermal conductivity, specific heat for ASTM A-106 GR B. Do you know where I can find it?

Thanks!!

R
 
Replies continue below

Recommended for you

Yes, the density is 0.284 lb/in3. The remaining physical properties can be found in ASME B&PV Code, Section II, Part D. If you do not have this section, see below

At 70 deg F

Thermal conductivity is 34.9 BTU/hr-ft-oF

Thermal Diffusivity is 0.700


TD = TC/[density x specific heat(BTU/lb-oF]

You can solve for the specific heat.
 
@metengr

Thank you very much. Just one question: in ASME section II part D can I find thermal conductivity and diffusivity at different temperatures?

Thanks!
 