Does anyone have the ID tolerance spec on 1-1/4" SCH 40 pipe?
Thanks!
 
Replies continue below

Recommended for you

It falls under an ASTM standard and an ASME standard...
 
There is no ID tol.
Only OD and wall tol.
You can see the total combined, and on pipe that is a big number.
The max wall on pipe is only limited by weight, so heavy pipe is a possibility.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 