Hi
Can anybody give me the proberties of ASTM A193 Gr. B7?

Especially, I need the modulus of elasticy.

Thank you very much

Claude
 
Replies continue below

Recommended for you

The modulus of elasticity is the typical value used for steels; 30 x 10^6 psi at ambient temperature.

The specified minimum mechanical properties are published in the ASTM Specification and are too cumbersome to state here because they are a function of diameter. I would suggest you review this ASTM specification.
 
CLAUDE47:

PLease review ASME II-A for the SA-193 specification. ASME II-D for the CODE allowable stresses, yeild and ultimate tensile stresses and modulus of elasticity. These CODES will be available with all pressure vessel engineers using ASME. All the above mentioned physical properties are a function of the temperature and size.