I work with a lot of B7 & B16 Studs and Bolts. I have the reference Chart on B7 which list bolt/stud size, nut size, minnimum Yeild Strenght PSI and various lubricants with torque reference based on the lubricant used. The charts I have are for 50% thru 70% Yields. I'm looking for the same in regarding B16 Material. If anyone could help me on this I would appreaciate.
 
I think you can use the same data for B7 and B16 since cold
Yield and Tensile are the same. B16 is only stronger at higher temperatures but this does not influence the bolting up condition.
 