In para. 8 of 234 is there a requirement to tensile strength a sample from each load of finsihed heat treated fittings when the the fittings are cold formed?
 
Replies continue below

Recommended for you

In the latest revision of this standard (2002), Chemical Composition is covered in Section 8 and Tensile Requirements in section 9. Section 9.2 requires 1 tensile test be performed on each heat of material, and Section 9.3 discusses the requirements for cold formed fittings.
 