CRES 304 CONDITION A

WHAT A DIFFRENT BETWEEN THIS 2 SPEC (ASTM A240 & QQ-S-763) FOR THE ABOVE MATERIAL?
 
Replies continue below

Recommended for you

Stainless steel 316/316L with related specs, ASTM A240, and AMS-QQ-S-763

which is ASTM A240 for sheet, strip and plate
AMS-QQ-S-763 for bar, wire and forging
 