I have a Russian spec which calls for valve body material as ASTM A352-LCC mod. Does anybody know what the qualifier "mod." implies? Is this material suitable for environmental temperatures of -60°C (-72°F)? I ask because the spec I see: ASTM A352 LCC (in the 2001 issue of Section II of the BPV code), specifies minimum testing temperature as -46°C or -50°F. At first sight I would have said it is not suitable, but I am not a materials engineer.
Thanks for your help in advance
I have a Russian spec which calls for valve body material as ASTM A352-LCC mod. Does anybody know what the qualifier "mod." implies? Is this material suitable for environmental temperatures of -60°C (-72°F)? I ask because the spec I see: ASTM A352 LCC (in the 2001 issue of Section II of the BPV code), specifies minimum testing temperature as -46°C or -50°F. At first sight I would have said it is not suitable, but I am not a materials engineer.