Is there a wrought equivalent in pipe for qualification of wps and welder for ASTM A487 A4,And which p group is it in Regards Gary

 
Replies continue below

Recommended for you

gtlord;
You can use AWS B2.1-2009 to obtain a Material-No. For
A 487 Grade 4, Class A, the AWS Material number would be;

M-No 10F
Group 1

Once you have the above, look for a similar wrought material with the same P-No and Group number.
 