I need to find an equivalent steel to ASTM A514 grade B in Europe. Can anyone suggest an online conversion site or does anyone know what could the equivalent be?
S690Q (1.8931) according to EN 10025-6 is the European equivalent. S690QL and S690QL1 have even better low temperature toughness. Here is a datasheet from Dillinger, one of the largest plate producers: