Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM A694 F60, looking for forging substitute in USA

Status
Not open for further replies.

jowens71

Mechanical
Mar 4, 2010
4
ASTM A694 F60 does not appear to be easily obtained in the USA. I’m looking for bar stock forging about 12" OD by 36" Long. Can anybody suggest an alternative?

Tensile yield = 60 ksi
Tensile strength = 75 ksi

Carbon Max = .30
Manganese Max = 1.5
Phosphorus Max = .030
Sulfur Max = .030
Silicon 0.13-0.37

The spec says ASTM A694 is used in high-pressure Transmission Service.