May 4, 2001 #1 caatd Materials May 4, 2001 1 0 0 US I am trying to build a C177 guarded hot plate test to measure the thermal conductivity of various insulation materials. Does anyone have any hints on building a simple but precise unit (or know of a good site to reference)?
I am trying to build a C177 guarded hot plate test to measure the thermal conductivity of various insulation materials. Does anyone have any hints on building a simple but precise unit (or know of a good site to reference)?
May 4, 2001 #2 Ron Structural Sep 24, 1999 16,336 0 36 US ASTM C1043 gives the design requirements for a guarded hot plate. You might also check the following website. It gives a schematic of the GHP. http://www.owlnet.rice.edu/~asteve/ Upvote 0 Downvote
ASTM C1043 gives the design requirements for a guarded hot plate. You might also check the following website. It gives a schematic of the GHP. http://www.owlnet.rice.edu/~asteve/